“…Due to the hydrophobic nature of the porous support layer [4], some suggest soaking membranes in a short-chain alcohol to ensure wetting prior to use [5,6,7]. Alcohols used for wetting are often ethanol and 2-propanol (or isopropyl alcohol, IPA), and contact times range from minutes to days [5,7,8,9,10,11,12,13]. However, the water permeance and salt rejection properties of TFC membranes can change after contact with these alcohols [5,7,8,9,10,11,12,13].…”