“…They state that “the single band at about 1225 cm -1 was observed also on silver and gold at a very low reducing potential”, i.e., below the region in which voltammetric studies show the prewave to commence. More recent studies at the VCCMP on the ethyl xanthate/silver system have demonstrated, however, that the band is absent at such potentials if care is taken to remove xanthate from the surface before exposure to the atmosphere. Thus, when the electrode surface was rinsed with deoxygenated xanthate-free solution immediately following opening of the circuit, the potential dependence of the intensity of the band closely paralleled that of voltammetric currents.…”