Our earlier results on ασ and heavy‐ion‐radiation damage in cellulose triacetate (CTA) are compared with those of previous authors on UV‐and γ‐radiation damage in the same material. Thus the common effects of these different methods of irradiation can be distinguished from those characteristic of the radiation employed. With heavy‐ion radiation the production of stable radicals is accompanied by C—O cleavage. In the case of 3684Kr (1 MeV/amu) ions, the number of free radicals produced is investigated, without distinguishing the species, by using the scavenger technique in the solid phase, combined with UV spectroscopy. On the other hand, C—O cleavage is observed by IR spectroscopy, with its inherent selectivity. A statistical study shows that the experimental curves representative of the evolution of the optical transmittance ratio before and after irradiation L(N) versus the ion fluence N are of exponential type:
where β is a parameter related to the volume damaged by a single ion and, therefore, to the latent track size. The latter is approximated by a cylinder whose height is equal to the range of the ion. For 3684Kr8+ (1.1 MeV/amu) the track length is 21 μ. For each type, damages are localized within a radius of 250 Å for free‐radical yields, 148 Å for cellulosic chain cleavages, 108 Å for deacetylation, and 100 Å for opening of pyrannosic rings. The track length is 14 μ for 1735Cl6+ (1 MeV/amu), while the radius of the cylinder in which free radicals are produced is only 80 Å.