Experimental Analysis of Al–TiC Sintered Nanocomposite on EDM Process Parameters Using ANOVA

Abstract: The size minimization of Titanium Carbide (TiC) Particles was done by high energy mechanical milling. Later Al & TiC powders were mixed to frame cylindrical preforms with 95% density using a die set. The cylindrical preform was sintered in a muffle

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
9
0

Year Published

2016
2016
2023
2023

Publication Types

Select...
8
2

Relationship

0
10

Authors

Journals

citations
Cited by 32 publications
(9 citation statements)
references
References 18 publications
0
9
0
Order By: Relevance
“…Excessive increase in the reinforcement content not only decreases the resistance of the composite's matrix, but also introduces more crack initiation's locations and eventually decreases the load-bearing capacity of the composite 25,26 . As it can be seen from figs.…”
Section: Resultsmentioning
confidence: 99%
“…Excessive increase in the reinforcement content not only decreases the resistance of the composite's matrix, but also introduces more crack initiation's locations and eventually decreases the load-bearing capacity of the composite 25,26 . As it can be seen from figs.…”
Section: Resultsmentioning
confidence: 99%
“…Sivaraj et al, [16] This research Proposed on Aluminum and Titanium Carbide powders with different particle sizes mixed and cylindrical composites by power metallurgy method and studies are carried out machining of EDM process. Using a copper tool, the composite was drilled by providing the tool negative polarization.…”
Section: P Sreeraj S Thirumalai Kumaran M Uthayakumar S Sureshmentioning
confidence: 99%
“…Further 1.5 h and later it was blended on a mass basis with 0, 5, 10 and 15%titanium carbide and rest aluminium powder. Then the combined Al/TiC powders were mixed scientifically in the high energy ball mill for another 0.25 h to attain homogeneous mixture [17].…”
Section: Powder Preparationmentioning
confidence: 99%