Factors Influencing Design of SMA Actuators

Abstract: Given the complex nonlinear nature of SMA responses, understanding their coupled thermomechanical responses of different components has been of significant interest for both researchers and application developers [1]. SMA component responses in different applications can be significantly affected by several factors like material compositions, component geometries, operating temperature, loading conditions, loading rates, thermomechanical history, processing conditions etc. and mostly combination of several of … Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
2

Citation Types

0
16
0

Year Published

2020
2020
2024
2024

Publication Types

Select...
5
1

Relationship

0
6

Authors

Journals

citations
Cited by 13 publications
(16 citation statements)
references
References 15 publications
0
16
0
Order By: Relevance
“…The best combination of geometrical parameters achieved was as follows: spring with an effective diameter of 10 mm built with a 1.5 mm diameter wire and assembled with three active coils. The springs are previously manufactured by shape setting (Lecce and Concilio, 2015; Rao et al, 2015). It is important to keep disk position and equivalent stiffness in order to ensure no changes in shaft height.…”
Section: Methodology and Experimental Developmentmentioning
confidence: 99%
See 4 more Smart Citations
“…The best combination of geometrical parameters achieved was as follows: spring with an effective diameter of 10 mm built with a 1.5 mm diameter wire and assembled with three active coils. The springs are previously manufactured by shape setting (Lecce and Concilio, 2015; Rao et al, 2015). It is important to keep disk position and equivalent stiffness in order to ensure no changes in shaft height.…”
Section: Methodology and Experimental Developmentmentioning
confidence: 99%
“…For thermal treatment ( 450 ° C for 25 min) (Figure 7(b)), the springs are covered with a thin sheet metal to prevent unwinding. After thermal treatment, helical springs as shown in Figure 7(c) are obtained (Rao et al, 2015).…”