an optical fiber and the circular polarization of the transmitted light was measured. The circular differential absorbance can then be calculated. Film thickness was determined using a Tencor P10 surface profilometer. AFM experiments were performed under ambient conditions in tapping mode. Microfabricated silicon cantilevers with a spring constant of 5 N m ±1 were used.