“…Until recently, it was assumed that Li2WO4 could not be grown by the Czochralski method due to the presence of a high-temperature phase transition. Therefore, a series of works on growing Li2WO4 doped with molybdenum [5,8,9], which showed the possibility of obtaining crystals with molybdenum content from 15 to 2.5%. Currently, the low-temperature heat capacity of lithium molybdate has been studied [10].…”