Glass-ceramic coating material for the CO 2 laser based sintering of thin films as caries and erosion protection

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

1
4
0

Year Published

2018
2018
2021
2021

Publication Types

Select...
6
1

Relationship

1
6

Authors

Journals

citations
Cited by 8 publications
(5 citation statements)
references
References 28 publications
1
4
0
Order By: Relevance
“…The literature 17,19,48,49 have shown that cerium did not alter bioactivity behavior when present in glass composition at low concentrations, which is in agreement with our resultshowever, none of them shown that low concentrations of rare earth could promote bioactivity. According to Borges et al, 21 the incorporation of rare earth elements (Gd and Yb) in the glass structure results in an increase of non-bridging oxygens despite their intermediate role in the glass structure, leading to a less connected glass network.…”
Section: Discussionsupporting
confidence: 93%
“…The literature 17,19,48,49 have shown that cerium did not alter bioactivity behavior when present in glass composition at low concentrations, which is in agreement with our resultshowever, none of them shown that low concentrations of rare earth could promote bioactivity. According to Borges et al, 21 the incorporation of rare earth elements (Gd and Yb) in the glass structure results in an increase of non-bridging oxygens despite their intermediate role in the glass structure, leading to a less connected glass network.…”
Section: Discussionsupporting
confidence: 93%
“…This shift may be associated with a possible formation of SiOP bonds, which would ensure a greater adhesion of the BG on the surface of the dentin as they would be chemically bonded to each other. A study carried out by Bilandzic et al () showed that BG ceramics can be chemically bonded to bovine enamel when CO 2 laser is applied. These findings indicated that chemical bonds between dentin and BGs might not have been excluded.…”
Section: Discussionmentioning
confidence: 99%
“…The XRF is used to test the composition of materials, the coating thickness, and to identify elements in dental materials: implant alloy [ 142 ] and ceramics [ 143 , 144 , 145 , 146 , 147 , 148 , 149 , 150 , 151 , 152 ]. XRD is used to obtain information of crystalline structure of solids such as dental ceramics [ 143 , 144 , 145 , 146 , 147 , 148 , 149 , 150 ].…”
Section: X-ray Spectroscopymentioning
confidence: 99%