Graphene/MnO2 composite prepared by a simple method for high performance supercapacitor

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
5

Citation Types

1
14
0

Year Published

2018
2018
2023
2023

Publication Types

Select...
6

Relationship

0
6

Authors

Journals

citations
Cited by 17 publications
(15 citation statements)
references
References 33 publications
1
14
0
Order By: Relevance
“…Graphite oxide, G, and NG all show the peak at 1720 cm −1 , which is ascribed to the C=O stretching. Another peak for G at 1214 cm −1 can be assigned to the C-O stretching [ 62 , 63 , 64 , 65 ]. For the N-containing composites (NG and x-NGM), the two main absorption peaks are at 1195 cm −1 and 1565 cm −1 , which are attributed to the C-N and C=N/C=C stretchings, respectively [ 66 , 67 ].…”
Section: Resultsmentioning
confidence: 99%
See 4 more Smart Citations
“…Graphite oxide, G, and NG all show the peak at 1720 cm −1 , which is ascribed to the C=O stretching. Another peak for G at 1214 cm −1 can be assigned to the C-O stretching [ 62 , 63 , 64 , 65 ]. For the N-containing composites (NG and x-NGM), the two main absorption peaks are at 1195 cm −1 and 1565 cm −1 , which are attributed to the C-N and C=N/C=C stretchings, respectively [ 66 , 67 ].…”
Section: Resultsmentioning
confidence: 99%
“…For graphite oxide and G, they have a strong energy peak centered at approximately 283.8 eV, which is assigned to the C=C bonds (sp 2 -hybridized carbon atoms). Another weak peak with higher binding energy at 285.6 eV can be assigned to the C-O bonds (oxygenated carbon atoms) [ 62 , 63 , 70 ]. There is a weaker peak for graphite oxide at 287.4 eV, which is assigned to the C=O bonds.…”
Section: Resultsmentioning
confidence: 99%
See 3 more Smart Citations