Graphite oxide/reduced graphite oxide surface modified carbon fiber reinforced composites for deicing and electromagnetic interference shielding

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1

Citation Types

0
3
0

Year Published

2023
2023
2024
2024

Publication Types

Select...
2

Relationship

0
2

Authors

Journals

citations
Cited by 2 publications
(3 citation statements)
references
References 31 publications
0
3
0
Order By: Relevance
“…The on/off response time of rGO layer to the applied voltage was 33.3 ms, as shown in the inset of Figure 4a, which satisfies the common conductor requirement with specific lightweight applications including long-range lightweight drones and flying object with electromagnetic interference shielding capability. [58][59][60][61][62][63] The origin of the fracture of 3D-printed object can be understood when the morphology of 3D-printed samples undergoes a mechanical tensile test. Three layers sequentially stacked, as shown in Figure 4e,f, show the weak point/linear contacts of filaments among layers and the continuous flow of the filament verifies the solid bonding behavior of pristine PLA itself.…”
Section: Resultsmentioning
confidence: 99%
See 1 more Smart Citation
“…The on/off response time of rGO layer to the applied voltage was 33.3 ms, as shown in the inset of Figure 4a, which satisfies the common conductor requirement with specific lightweight applications including long-range lightweight drones and flying object with electromagnetic interference shielding capability. [58][59][60][61][62][63] The origin of the fracture of 3D-printed object can be understood when the morphology of 3D-printed samples undergoes a mechanical tensile test. Three layers sequentially stacked, as shown in Figure 4e,f, show the weak point/linear contacts of filaments among layers and the continuous flow of the filament verifies the solid bonding behavior of pristine PLA itself.…”
Section: Resultsmentioning
confidence: 99%
“…The on/off response time of rGO layer to the applied voltage was 33.3 ms, as shown in the inset of Figure 4a, which satisfies the common conductor requirement with specific lightweight applications including long‐range lightweight drones and flying object with electromagnetic interference shielding capability. [ 58–63 ]…”
Section: Resultsmentioning
confidence: 99%
“…Modified sensor materials are used in various systems including electrochemical, batteries, and biosensors, etc. [ [25] , [26] , [27] , [28] , [29] , [30] , [31] ].…”
Section: Introductionmentioning
confidence: 99%