Highly conductive, ultra-flexible and continuously processable PEDOT:PSS fibers with high thermoelectric properties for wearable energy harvesting

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

2
104
0

Year Published

2021
2021
2024
2024

Publication Types

Select...
7
1
1

Relationship

2
7

Authors

Journals

citations
Cited by 135 publications
(106 citation statements)
references
References 66 publications
2
104
0
Order By: Relevance
“…(G) TEM image of PEDOT: PSS films with 6 wt% Cu-Bi 0.5 Sb 1.5 Te 3 filler incorporation; (H) images of the as-fabricated F-TE, and its thermovolta2021/9/29ge generations with human wrist and chest as thermal sources; (I) measured thermovoltage using a heating plate, human wrist, and chest as thermal sources. Reproduced with permission [204] . Copyright 2020 ELSEVIER.…”
Section: Pedot: Pssmentioning
confidence: 99%
See 1 more Smart Citation
“…(G) TEM image of PEDOT: PSS films with 6 wt% Cu-Bi 0.5 Sb 1.5 Te 3 filler incorporation; (H) images of the as-fabricated F-TE, and its thermovolta2021/9/29ge generations with human wrist and chest as thermal sources; (I) measured thermovoltage using a heating plate, human wrist, and chest as thermal sources. Reproduced with permission [204] . Copyright 2020 ELSEVIER.…”
Section: Pedot: Pssmentioning
confidence: 99%
“…In addition to pure PEDOT: PSS thin films, the hybrids of organic and inorganic materials have improved TE performance. For example, a thin-film material with high crystallinity was obtained by combining Bi 0.5 Sb 1.5 Te 3 (BST) and PEDOT: PSS [204] . Figure 8G is a TEM image of BST-modified PEDOT: PSS.…”
Section: Pedot: Pssmentioning
confidence: 99%
“…The generator produced an output voltage of 45.2 mV and output power of 375 μW at a temperature difference of 60 K [ 89 ]. The PEDOT:PSS fibers, prepared by a continuous wet-spinning process, were treated with sulfuric acid, which had effective modulation on composition and chain conformation, as shown in Figure 5 a,b [ 96 ]. Under optimal conditions, PEDOT: PSS fibers delivered a Seebeck coefficient of 19.2 μVK −1 and a power factor of 147.8 μWm −1 K −2 [ 96 ].…”
Section: Organic Te Fibermentioning
confidence: 99%
“…Reproduced with permission [242] . (f) The reported maximum ZT (ZTmax) for the fiber-based thermoelectric materials in recent years [243][244][245][246][247][248][249][250][251][252][253][254][255]. Reproduced with permission.…”
Section: Fan Assisted Garmentmentioning
confidence: 99%