“…The pure PCMs (TDA, HDA, and ODA), CuOHS@PCMs, and CuOHS exhibit different thermal stability under 0–600 °C air environment, respectively. As shown in the TG curve in Figure a,b, the temperature at 100% weight loss of the three aliphatic amines gradually increases as the chain length of the aliphatic amine increases . For CuOHS, it showed excellent thermal stability compared to the other samples, maintaining a mass of 82.57% at 600 °C and a weight loss of 100% for the pure PCM, while CuOHS@PCMs maintained a mass of 46.31, 39.71, and 39.33% at 600 °C, respectively.…”