“…For the CYAGO:Eu samples synthesized above 950 • C, seven emission bands are observed at 581 nm, 591 nm, 599 nm, 622 nm, 657 nm, 693 nm, and 702 nm. These emission bands are associated with the transitions of 5 D 0 → 7 F 0 (581 nm), 5 D 0 → 7 F 1 (591 and 599 nm), 5 D 0 → 7 F 2 (622 nm), 5 D 0 → 7 F 3 (657 nm), and 5 D 0 → 7 F 4 (693 and 703 nm), respectively [20,30,31]. The PL intensities gradually increase with increasing the synthesis temperature, which is attributed to the improvement in crystallinity and/or the change in the local environment around Eu ions following Ga substitution.…”