“…[ 17 ] This fabrication process is scalable, as demonstrated by the recent development of large-area synthesis of SWNT forests. [ 18 ] For comparison, AC electrode sheets (density 0.6 g cm − 3 , area 1 cm 2 , thickness ca. 100 μ m) were also made by a conventional process, that is, mixing and kneading of AC powder (YP17: 1640 m 2 g − 1 ) with a binder (poly(tetrafl uoroethylene), PTFE) and a conducting agent (carbon black).…”