“…1 The observed heat of mixing was positive when mixing the main atomic pairs (13 and 9 kJ·mol -1 when mixing the La-Zr and Zr-Gd atomic pairs, respectively), although both pairs may yield negative heat values when mixed with others (e.g., the La(Zr)-Al, La(Zr)-Cu, La(Zr)-Ni atomic pairs, or the Zr(Gd)-Al, Zr(Gd)-Co atomic pairs). 1,3 However, the phase separation observed for La-Zr-and Zr-Gd-based alloys is stronger than that observed for the alloys with the negative heat obtained from the mixing of the main atomic pairs, and this can be detected experimentally by scanning electron microscopy (SEM) and transmission electron microscopy (TEM). 1,3 For MG with a high glass forming ability (GFA), the heat of mixing is negative when mixing the main atomic pairs (e.g., the La-Al, La-Cu, La-Ni and La-Co atomic pairs in La-Al-Cu-Ni(Co) alloy systems) and the phase separation is weak.…”