Abstract:The paper focuses on the assessment of the hull girder ultimate strength, combined with random pitting corrosion wastage, by the incremental-iterative method. After a brief review about the state of art, the local ultimate strength of pitted platings under uniaxial compression is preliminarily outlined and subsequently a closed-form design formula is endorsed in the Rule incremental-iterative method, to account for pitting corrosion wastage in the hull girder ultimate strength check. The ISSC bulk carrier is a… Show more
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.