Influence of different melt processings upon the microstructure and critical current of textured Y123

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
9
0

Year Published

1998
1998
2015
2015

Publication Types

Select...
8
1

Relationship

0
9

Authors

Journals

citations
Cited by 20 publications
(9 citation statements)
references
References 36 publications
0
9
0
Order By: Relevance
“…The average size of the YBaTa phase is about 4.2 (7 0.3) μm. It is well known that an intragranullar doping effectively acts as a pinning center [32]. The micrograph of the sample with 4 wt% of YBaTa shows the Y 2 BaCuO 5 (Y211) phase segregation.…”
Section: Resultsmentioning
confidence: 99%
“…The average size of the YBaTa phase is about 4.2 (7 0.3) μm. It is well known that an intragranullar doping effectively acts as a pinning center [32]. The micrograph of the sample with 4 wt% of YBaTa shows the Y 2 BaCuO 5 (Y211) phase segregation.…”
Section: Resultsmentioning
confidence: 99%
“…Such reactions consume the 211 phase to form the 123 superconducting phase which inherently leads to the incorporation of a finer and much more homogeneous dispersion of 211 particles in the matrix as 123 grains grow within the films. Equivalent improvements in both the grain growth characteristics and the distribution of second-phase 211 particles have previously been observed in the processing of bulk YBCO materials by the PMP and SLMG routes [26][27][28][29].…”
Section: Microstructural Analysismentioning
confidence: 85%
“…The nominal composition corresponds to the final phase composites of Y123 + 0.4 Y211, which is widely believed to be an optimum ratio for refining of Y211 precipitates, hindering of liquidphase loss, improvement of stable morphologies, and enhancement of flux pinning. 1,17,18 After calcination in air at 900°C for 30 h with an intermediate grinding, the powders of 10 wt% Ag 2 O and 0.5 wt% Pt were added. The resultant powder was uniaxially pressed into a pellet 20 mm in diameter and 7 mm in thickness.…”
Section: Methodsmentioning