Influence of Different Preparation Designs on Fracture Strength of Porcelain Laminate Veneer

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1

Citation Types

0
2
0

Year Published

2020
2020
2022
2022

Publication Types

Select...
2

Relationship

0
2

Authors

Journals

citations
Cited by 2 publications
(2 citation statements)
references
References 0 publications
0
2
0
Order By: Relevance
“…An autopolymerized acrylic resin material was used as a base to fix each metal die 1 mm apical to the CEJ to simulate the natural biologic width and the base was held in a metallic mold (Chai et al, 2020 ; Gupta et al, 2018 ; Tomer et al, 2018 ).…”
Section: Methodsmentioning
confidence: 99%
“…An autopolymerized acrylic resin material was used as a base to fix each metal die 1 mm apical to the CEJ to simulate the natural biologic width and the base was held in a metallic mold (Chai et al, 2020 ; Gupta et al, 2018 ; Tomer et al, 2018 ).…”
Section: Methodsmentioning
confidence: 99%
“…On the other hand, gupta 13 etal in 2018 had reported the fracture strength of e-max press laminate veneer of different designs. It ranged from 920 N to 1503 N. This variation in results could be attributed to difference in the designs.…”
Section: Shimaa Elmetwally Sabermentioning