2009
DOI: 10.1016/j.wear.2008.05.009
|View full text |Cite
|
Sign up to set email alerts
|

Influence of electrical discharge machining on the reciprocating sliding wear response of WC-Co cemented carbides

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

3
11
0
3

Year Published

2014
2014
2024
2024

Publication Types

Select...
4
1
1

Relationship

1
5

Authors

Journals

citations
Cited by 31 publications
(17 citation statements)
references
References 20 publications
3
11
0
3
Order By: Relevance
“…7, the wear volume loss is inversely proportional to the bulk hardness of the WC-Ni grades, in agreement with e.g. [29,32,33,41,42]. This can be attributed to more pronounced adhesion and micro-abrasion for the lowest hardness WC-Ni alloys.…”
Section: Discussionsupporting
confidence: 81%
See 1 more Smart Citation
“…7, the wear volume loss is inversely proportional to the bulk hardness of the WC-Ni grades, in agreement with e.g. [29,32,33,41,42]. This can be attributed to more pronounced adhesion and micro-abrasion for the lowest hardness WC-Ni alloys.…”
Section: Discussionsupporting
confidence: 81%
“…The wear level of both grade-A and grade-B samples is considerably higher compared to grade-C. The very low wear for grade-C is commensurate with the lower friction level for this grade and should be related to the higher hardness (see Table 1) and/or lower binder content compared to the other grades [29,32,33]. …”
Section: Online Wear Monitoringmentioning
confidence: 72%
“…Para esto se utilizó como máquina de ensayos un tribómetro desarrollado por MICROTEST, modelo MT2/60/SCM/T que responde a lo propuesto en la norma ASTM G99-03 [113].…”
Section: Equipamiento Y Procedimiento Experimentalunclassified
“…Proporciona además el perfil de la superficie que ha sido analizada, impreso en papel. La norma ASTM G99-03 [113] recomienda que los ensayos de desgaste por deslizamiento en seco se realicen en materiales con una rugosidad superficial R a de 0.8 μm como límite superior.…”
Section: Rugosidad Superficialunclassified
See 1 more Smart Citation