Influence of forging and heat treatment on wear properties of Al–Si and Al–Pb bearing alloys in oil lubricated conditions

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
11
0

Year Published

2015
2015
2024
2024

Publication Types

Select...
9
1

Relationship

0
10

Authors

Journals

citations
Cited by 30 publications
(11 citation statements)
references
References 30 publications
0
11
0
Order By: Relevance
“…Parallel to the rapidly developing technology, expectations of the qualification of materials are also increasing. Over the several past decade's grain refinement has been mostly applied for enhancing the microstructural and mechanical properties of aluminum alloys through physical and chemical methods such as severe plastic deformation, mechanical alloying, conventional thermomechanical processing, and adding grain refiners [1][2][3][4][5]. Ultrasonic vibration (20 kHz-1 GHz frequencies) application is a relatively new method compared to the other methods used to improve the mechanical properties of materials.…”
Section: Introductionmentioning
confidence: 99%
“…Parallel to the rapidly developing technology, expectations of the qualification of materials are also increasing. Over the several past decade's grain refinement has been mostly applied for enhancing the microstructural and mechanical properties of aluminum alloys through physical and chemical methods such as severe plastic deformation, mechanical alloying, conventional thermomechanical processing, and adding grain refiners [1][2][3][4][5]. Ultrasonic vibration (20 kHz-1 GHz frequencies) application is a relatively new method compared to the other methods used to improve the mechanical properties of materials.…”
Section: Introductionmentioning
confidence: 99%
“…3b. This gure also shows some of the Al 3 Zr precipitates located at the grain boundaries with other intermetallics which are mainly Al-Fe-Si phases in the Al-Zr alloy [12]. Taking place at boundaries of Al 3 Zr was veried by EDS patern in Fig.…”
Section: Resultsmentioning
confidence: 94%
“…The minor Cu addition to the A356 alloy transforms the a-Al coarse dendritic structure into the equiaxed structure as elongated grain size reduced wear rate. Feyzullahog˘lu et al 88 assessed mechanical properties of Al-Si and Al-Pb alloys by heat treatment and forging effect. Normally in the heat treatment process, grain growth hardness was decreased then followed by forging means strain-induced which control the grain growth.…”
Section: Effect Of Intermetallic Phases On Properties Of Al Alloysmentioning
confidence: 99%