Abstract:Potential-induced degradation (PID) was observed for crystalline Si photovoltaic (PV) modules set at a PID test system constructed outdoors. It was clearly shown that partial shadow and periodical water spray during daytime accelerate PID generation. PID easily occurred just underneath the shielding plate. It was also found that when a large part of one cell in the PV module was shadowed, PID is accelerated; however, when a small part of one cell in the PV module was shadowed or when the weak light is uniforml… Show more
Set email alert for when this publication receives citations?
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.