“…The composite reached its peak hardness in shorter time compared with the unreinforced alloy on solution treatment for 2 and 3 h, but reached it in longer time on solution heat treatment for 1 h (Mosuavi & Seyed, 2010). Using the same alloy type, 2124, Thomas and King studied the formation of phases during precipitation by differential scanning calorimetry (DSC) (Thomas & King, 1994 (Cottu et. al., 1992).…”