“…Limited isothermal oxidation studies on RuAl alloys have shown relatively good oxidation resistance up to 1000 C [2,4,5,14]. Soldera and co-workers reported that single phase RuAl produced by reactive sintering showed excellent oxidation resistance at 1000 C due to the formation of a dense, protective Al 2 O 3 scale [14]. Conversely, a porous and discontinuous a-Al 2 O 3 scale was formed during isothermal oxidation of an arc-melted near-stoichiometric RuAl alloy, due to the vaporization of the Ru oxides at 1000 C [15].…”