2018
DOI: 10.1016/j.jallcom.2017.10.212
|View full text |Cite
|
Sign up to set email alerts
|

Influences of metastable θ″, θ′ and stable θ intermetallics formed during cryorolling and friction stir welding process on AA2219

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
5
0

Year Published

2018
2018
2023
2023

Publication Types

Select...
7
1
1

Relationship

0
9

Authors

Journals

citations
Cited by 12 publications
(5 citation statements)
references
References 18 publications
0
5
0
Order By: Relevance
“…The grain boundaries of the LNR50U and LNR50C alloy are not clearly visible, as in the T87 condition, due to the heavy deformation of the alloy during the rolling process. The cryorolled material exhibits a cellular structure due to higher plastic deformation when compared with the RTR material 16 . The extent of cellular structure and fragmented grains is maximum in the LNR50C cross rolled alloys when compared with the other rolled condition.…”
Section: Resultsmentioning
confidence: 97%
“…The grain boundaries of the LNR50U and LNR50C alloy are not clearly visible, as in the T87 condition, due to the heavy deformation of the alloy during the rolling process. The cryorolled material exhibits a cellular structure due to higher plastic deformation when compared with the RTR material 16 . The extent of cellular structure and fragmented grains is maximum in the LNR50C cross rolled alloys when compared with the other rolled condition.…”
Section: Resultsmentioning
confidence: 97%
“…Further, Noor et al [16] reported AA2219 and AA7475 dissimilar aluminum alloy and observed that in nugget zone there is a lot of grain refinement. Kamalbabu et al [17] reported FSW study on AA2219/PP and evidenced irregular shape area and a minor interfacial irregularity may be observed in the thread hole of the hybrid AA2219/PP interface. Anderson et al [18] 2219-T87 a combination of plasticity induced crack and uneven crack propagation rates of the base material were related to roughness-induced cracks.…”
Section: Journal Of Mines Metals and Fuelsmentioning
confidence: 99%
“…In addition, the solid solubility of Cu would be increased in ultrasonic conditions, which acted as a pining effect to increase the strength of the Al alloy during the deformation process. Moreover, due to the difference in atomic matching between Cu and Al, the dislocation density would be increased with the increase in Cu content in the Al matrix, which increases the ability of the material to resist deformation and enhance the strength [41]. When the eutectic phase area fraction was high with DC, the eutectic phase Al 2 Cu hardness value was higher than that of the Al matrix [42].…”
Section: Effect Of Ultrasonic Treatment On Mechanical Propertiesmentioning
confidence: 99%