2016
DOI: 10.1016/j.micromeso.2016.07.008
|View full text |Cite
|
Sign up to set email alerts
|

Innovative layer by layer and continuous growth methods for synthesis of ZIF-8 membrane on porous polymeric support using poly(ether- block -amide) as structure directing agent for gas separation

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

4
43
0

Year Published

2017
2017
2024
2024

Publication Types

Select...
7

Relationship

0
7

Authors

Journals

citations
Cited by 76 publications
(47 citation statements)
references
References 47 publications
4
43
0
Order By: Relevance
“…It presented remarkable bands at 3455, 3135, 2929, 1635, 1585, 1458, 1425, 1385, 1309, 1146, 995, 760, 694 and 426 cm À1 for ZIF-8 sample. These FT-IR bands were consistent with those previously reported by Cravillon et al, Ordonez et al and Jomekian et al [35][36][37] The band at 3455 cm À1 might be attributed to the N-H stretching vibration of the residual Hmim and the O-H stretching vibration of water from KBr deliquescence. The peaks at 3135 and 2929 cm À1 were associated with the aromatic and aliphatic C-H asymmetric stretching vibrations, respectively.…”
Section: Ftir Spectroscopy Analysissupporting
confidence: 91%
“…It presented remarkable bands at 3455, 3135, 2929, 1635, 1585, 1458, 1425, 1385, 1309, 1146, 995, 760, 694 and 426 cm À1 for ZIF-8 sample. These FT-IR bands were consistent with those previously reported by Cravillon et al, Ordonez et al and Jomekian et al [35][36][37] The band at 3455 cm À1 might be attributed to the N-H stretching vibration of the residual Hmim and the O-H stretching vibration of water from KBr deliquescence. The peaks at 3135 and 2929 cm À1 were associated with the aromatic and aliphatic C-H asymmetric stretching vibrations, respectively.…”
Section: Ftir Spectroscopy Analysissupporting
confidence: 91%
“…40 and Jomekian et al . 41 . The band at 3455 cm −1 might be attributed to the N–H stretching vibration of the residual Hmim and the O–H stretching vibration of water from KBr deliquescence.…”
Section: Resultsmentioning
confidence: 99%
“…2(D). 11,15 When using this technique, the polymeric substrate was first immersed in a precursor solution containing the metal ions. It was then subsequently immersed in a ligand precursor solution, followed by washing and drying.…”
Section: In Situ Growing Methodsmentioning
confidence: 99%
“…The simplest strategy to grow ZIF‐8 membrane based on this method is to directly immerse the polymeric substrate into MOF precursor solutions. Various polymers have been investigated using this approach, such as polysulfone (PSF), polyphenylsulfone (PPSU) and polyimide (PI) . In this approach, controlling the synthesis condition is important since it will affect both the particle size of the ZIF‐8 and the final membrane structure .…”
Section: Fabrication Strategies Of Zif‐8 Membranes On Polymeric Substmentioning