“…As the characterization of the LBE-affected Zr2AlC grains revealed the local formation of a new Zr2(Al,Bi,Pb)C MAX phase solution [13], it was decided to synthesize this new MAX phase solid solution by reactive hot pressing for detailed structural characterization. For this purpose, ZrH2 (grain size <6 μm, >99% purity, Chemetall, Germany), LBE (44.5 wt% Pb and 55.5 wt% Bi, MCP 124, 5N Plus Lübeck GmbH, Belgium), Al (<5 μm, >99% purity, AEE, USA), and C (<5 μm, >99% purity, Asbury Graphite Mills, USA) powders were mixed in Zr:Al:LBE:C 2:0.55:0.55:0.95.…”