Investigation of the suitability of commercially available CVD diamond for megavoltage X-ray dosimetry

Abstract: Sandwich-type x-ray detectors were fabricated on commercially-available chemical vapour deposition diamond sourced from three manufacturers: Diamond Materials GmbH, Diamonex, and Element Six. These devices were investigated using Raman spectroscopy and 6 megavolt photons from a clinical linear accelerator. Parameters such as the level of the dark (leakage) and photo-currents, necessary priming dose, linearity of photocurrent with dose rate, and device sensitivity were considered. Device characteristics vary co… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1

Citation Types

0
4
0

Year Published

2010
2010
2021
2021

Publication Types

Select...
7

Relationship

1
6

Authors

Journals

citations
Cited by 21 publications
(4 citation statements)
references
References 29 publications
0
4
0
Order By: Relevance
“…A considerable progress in diamond growth has recently been achieved due to the adaptation of the chemical vapour deposition (CVD) method to the growth of high-quality single crystal diamond films [9][10][11][12]. In this process, high pressure high temperature (HPHT) single crystals with a special orientation are usually used as a substrate or seed.…”
Section: Introductionmentioning
confidence: 99%
“…A considerable progress in diamond growth has recently been achieved due to the adaptation of the chemical vapour deposition (CVD) method to the growth of high-quality single crystal diamond films [9][10][11][12]. In this process, high pressure high temperature (HPHT) single crystals with a special orientation are usually used as a substrate or seed.…”
Section: Introductionmentioning
confidence: 99%
“…It is possible, for example, to understand if the crystal structure is pure (peak at 1,332.8 cm -1 ) or if there are other contributions due to vacancies that could act as a trapping center for charges (other peaks). For the pcCVD substrate, the level of defects could also depend on the large concentration of grain boundaries [46][47][48][49]. This analysis is sometimes complemented by optical spectrophotometry or FTIR methods to detect substitutional defects in the diamond lattice.…”
Section: Characterization Techniquesmentioning
confidence: 99%
“…This detector contains an air cavity around the diamond crystal; the diameter of this cavity is about 6 mm. Further details of the detector fabrication, including contacts, bonding and encapsulation, can be found in [13]. The diamond film used in this detector was a commercially-available synthetic diamond film manufactured by CVD [19]; details of this film are listed in Table 1.…”
Section: Detectorsmentioning
confidence: 99%
“…At the University of Canterbury, we have been fabricating and characterising X-ray detectors from commercially-available synthetic diamond films [13][14][15]. In this paper we present a comparison between one of these synthetic diamond X-ray detectors and a commercial natural diamond detector.…”
Section: Introductionmentioning
confidence: 99%