Abstract:The preparation process of porous Cu35Ni15Cr alloy was studied in this paper. The effect of ball milling time and sintering temperature on the porosity of Cu35Ni15Cr alloy was identified. It was found that 18 h ball milling and 950°C sintering are the most promising parameters for the preparation of porous Cu35Ni15Cr alloy. The products have a ∼62 % porosity. The alloy consists of an α phase and β phase. The influence of deformation temperature and loading rate on the mechanical properties of Cu35Ni15Cr alloys… Show more
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.