K0.5Na0.5VO3-SiO2 Co-sintering Agent of Ceramic Mg0.8Ti0.2O3 as Dielectric Material Candidate
Sefrilita Risqi Adikaning Rani,
Ika Widya Wahyuningsih,
Cindi Regita Cahyani
Abstract:This paper focuses on the characteristics of K0.5Na0.5VO3 (KNV) and SiO2 when added to Mg0.8Zn0.2TiO3 (MZT) material to reduce the sintering temperature. Initially, a single phase of Mg0.8Zn0.2TiO3 (MZT) was synthesized using the conventional solid-state reaction method at 850°C for 4 hours. Subsequently, (K0.5Na0.5)VO3 was formed as a single phase at a temperature of 500°C for 2 hours. The reduction of MZT sintering temperature was then carried out by adding K0.5Na0.5VO3 and SiO2 and sintering at 950°C for 4 … Show more
Set email alert for when this publication receives citations?
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.