Kinetics of Langbeinite Conversion into Schenite in the Presence of Mirabilite, Sylvine and Water

Abstract: The conversion of langbeinite into schenite has been investigated under isothermal conditions within 273-333 K in the presence of mirabilite, sylvine and water. The reaction rate has been determined at various temperatures and "apparent" activation energy has been examined within 293-303 K. The reaction order by langbeinite has been determined as well.

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1

Citation Types

0
1
0
1

Year Published

2017
2017
2020
2020

Publication Types

Select...
3

Relationship

1
2

Authors

Journals

citations
Cited by 3 publications
(2 citation statements)
references
References 1 publication
0
1
0
1
Order By: Relevance
“…Щоб не допустити утворення відхідних розчинів магнію хлориду, запропоновано вводити у перероблювані системи натрію сульфат, що зв'язуватиме надлишковий магній у магнію сульфат [4][5][6][7][8][9], який можна випускати як окремий продукт або вводити до складу добрив.…”
Section: вступunclassified
“…Щоб не допустити утворення відхідних розчинів магнію хлориду, запропоновано вводити у перероблювані системи натрію сульфат, що зв'язуватиме надлишковий магній у магнію сульфат [4][5][6][7][8][9], який можна випускати як окремий продукт або вводити до складу добрив.…”
Section: вступunclassified
“…There is a known method according to which the natural kainite purified from sodium chloride under industrial conditions is converted into schoenite in the schoenite solution at ambient temperature [3]. Schoenite crystallization is also used for the conversion of langbeinite and kieserite with potassium chloride and natural mirabilite into schoenite [4].…”
Section: Introductionmentioning
confidence: 99%