“…The authors of [177] performed the growth of MWCNTs by the laser-assisted CVD method using C 2 H 4 as carbon source (Ar and H 2 were used as gas carriers) and Fe catalyst at temperatures of 600–1000 °C. Varying the concentration of C 2 H 4 allowed changing the activation energy between the values of 0.25 eV, which was assigned to the adsorption of gaseous carbon source on the catalyst particle, 0.36 eV, which corresponded to the mass diffusion of the carbon source, 0.57 eV, which was assigned to the dissociation of the carbon precursor to carbon, and 0.76 eV, which corresponded to the surface diffusion of carbon on the catalyst particle.…”