Kinetics of thermal degradation of raw lacquer enhanced by formaldehyde urea prepolymer

Abstract: In this study, formaldehyde-urea prepolymer (FUP) were synthesized, which were used to modify the raw lacquer (RL) and this composition named LF, while the basic properties of the RL were tested. Thermal gravimetric (TG) analysis and scanning electron microscopy (SEM) were used to analyze the degradative characteristics and the surface morphology of RL before and after modification. The result indicated that FUP can significantly improve the performance of RL. The drying time of the LF is significantly shorten… Show more

Help me understand this report
View preprint versions

Search citation statements

Order By: Relevance

Paper Sections

Select...

Citation Types

0
0
0

Year Published

2024
2024
2024
2024

Publication Types

Select...
2

Relationship

0
2

Authors

Journals

citations
Cited by 2 publications
references
References 43 publications
0
0
0
Order By: Relevance