“…Previous studies [18,19] using X-ray CT highlighted the importance of taking the 3D aspect into account when considering the UD fibre fractures of quasi-UD NCF based composites. X-ray CT has been successfully used to monitor damage in fibre composites in several studies [18,19,[21][22][23][24][25][26][27][28][29][30][31][32][33][34], however it has the general disadvantage that cracks with an opening smaller than the resolution will not be visible (usually the voxel size is larger than 1µm). As a result, X-ray CT studies generally consider small specimens to obtain sufficient image resolution.…”
Section: Fatigue Damage Mechanisms Of Fibre Compositesmentioning
“…Previous studies [18,19] using X-ray CT highlighted the importance of taking the 3D aspect into account when considering the UD fibre fractures of quasi-UD NCF based composites. X-ray CT has been successfully used to monitor damage in fibre composites in several studies [18,19,[21][22][23][24][25][26][27][28][29][30][31][32][33][34], however it has the general disadvantage that cracks with an opening smaller than the resolution will not be visible (usually the voxel size is larger than 1µm). As a result, X-ray CT studies generally consider small specimens to obtain sufficient image resolution.…”
Section: Fatigue Damage Mechanisms Of Fibre Compositesmentioning
“…These systems make it easier to perform multiple longer timescale studies, albeit using much longer scan times compared to synchrotron CT. Since laboratory X-ray CT systems capable of micro resolution have only recently emerged, only a few studies to date [12,[22][23][24][25] have used laboratory systems to study material damage at the micro-structural level. The studies have tended not to consider individual fibre fractures because of insufficient resolution (e.g.…”
Section: X-ray Ct Of Damage In Compositesmentioning
Users may download and print one copy of any publication from the public portal for the purpose of private study or research. You may not further distribute the material or use it for any profit-making activity or commercial gain You may freely distribute the URL identifying the publication in the public portal If you believe that this document breaches copyright please contact us providing details, and we will remove access to the work immediately and investigate your claim.
“…-the longitudinal elastic moduli, Ey ch , is defined from the data points of the first stages of traction using the method reported in [27]: a chord modulus is calculated as the slope of a straight line fitting the corrected machine data points over the strain range 0.03%-0.13%. The secant properties are generally strongly affected by creep effects, so corrected data on movable head displacement have been used for "elastic" properties calculation; -the longitudinal secant moduli, Ey ch Ey sec , has been calculated using the maximum longitudinal strain and the maximum longitudinal stress values for each load/unload cycle; -the hysteresis area, A, is used to characterize the load/unload cycles in full, while the previous two properties characterize only the load stage.…”
Section: -Materials and Experimental Approachmentioning
confidence: 99%
“…This last value is kept until the end of the test for the air and 2 bar N2 specimen, while a slightly rise is seen for the 2 bar O2 specimen just before the failure. This final rise for the 2 bar O2 specimen, could be due to the stick-slip frictional sliding ( [27], [28]).…”
Section: -Property Evolution During Fatiguementioning
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.