2022
DOI: 10.3390/nano12101706
|View full text |Cite
|
Sign up to set email alerts
|

Long-Term Exposure of MoS2 to Oxygen and Water Promoted Armchair-to-Zigzag-Directional Line Unzippings

Abstract: Understanding the long-term stability of MoS2 is important for various optoelectronic applications. Herein, we show that the long-term exposure to an oxygen atmosphere for up to a few months results in zigzag (zz)-directional line unzipping of the MoS2 basal plane. In contrast to exposure to dry or humid N2 atmospheres, dry O2 treatment promotes the initial formation of line defects, mainly along the armchair (ac) direction, and humid O2 treatment further promotes ac line unzipping near edges. Further incubati… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1

Citation Types

0
4
0

Year Published

2022
2022
2024
2024

Publication Types

Select...
4

Relationship

2
2

Authors

Journals

citations
Cited by 4 publications
(4 citation statements)
references
References 51 publications
0
4
0
Order By: Relevance
“…The scattering image, illuminated at each excitation wavelength (λ), is captured by a CCD camera through a dark-field lens that selectively collects scattering light while rejecting reflected light. Figure B presents a schematic representation of an image stack that features a triangular MoS 2 grain on a quartz substrate, obtained by dry transfer of the synthesized grain using the conventional chemical vapor deposition (CVD) method as outlined in our previous reports , (Methods). The image stack (see the movie), which combines images excited at each λ ranging from 430 to 800 nm, contains both spatial and spectral information.…”
Section: Resultsmentioning
confidence: 99%
See 2 more Smart Citations
“…The scattering image, illuminated at each excitation wavelength (λ), is captured by a CCD camera through a dark-field lens that selectively collects scattering light while rejecting reflected light. Figure B presents a schematic representation of an image stack that features a triangular MoS 2 grain on a quartz substrate, obtained by dry transfer of the synthesized grain using the conventional chemical vapor deposition (CVD) method as outlined in our previous reports , (Methods). The image stack (see the movie), which combines images excited at each λ ranging from 430 to 800 nm, contains both spatial and spectral information.…”
Section: Resultsmentioning
confidence: 99%
“…After the furnace temperature reached 750 °C, the crucible was kept at 750 °C for 20 min and then cooled under the argon flow until the temperature reached 100 °C (20 min). The growth of MoS 2 was achieved using the previously developed method , involving the CVD method with spin-coated MoO 3 and S as precursors [Figure S1A and S1B for the CVD apparatus and the schematic of CVD growth, respectively]. Optical images (Figure S1C–S1D) reveal that most of the MoS 2 formed has a triangular shape, showing an average size of 12 μm 2 (Figure S1E).…”
Section: Methodsmentioning
confidence: 99%
See 1 more Smart Citation
“…Micro Raman measurements were conducted using a custom-made instrument equipped with a 532 nm laser (Cobolt 08-DPL, Hubner Photonics) via a backscattering geometry according to the previous literature. Briefly, inelastic scattering signals from the focused laser spot on the sample were collected via an objective lens (50× or 100×, Plan, Olympus, Japan) in an upright microscope (BX51, Olympus, Japan). The collected scattering was focused via a tube lens in a trinocular of the microscope and dispersed and recorded with a spectrometer (Triax320, Horiba, Japan) with 1800 g/mm (resolution < 1 cm –1 ) and a charge-coupled device detector (Synergy, Horiba, Japan).…”
Section: Methodsmentioning
confidence: 99%