Low Temperature Zinc Indium Oxide Backplane Development for Flexible OLED Displays in a Manufacturing Pilot Line Environment

Abstract: A low temperature amorphous zinc indium oxide (ZIO) thin film transistor (TFT) backplane technology for high information content flexible organic light emitting diode (OLED) displays has been developed. We have fabricated 4.1-in. diagonal OLED backplanes on the Flexible Display Center’s six-inch wafer-scale pilot line using ZIO as the active layer. The ZIO based TFTs exhibited an effective saturation mobility of 18.6 cm2/V-s and a threshold voltage shift of 2.2 Volts or less under positive and negative gate bi… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...

Citation Types

0
0
0

Publication Types

Select...

Relationship

0
0

Authors

Journals

citations
Cited by 0 publications
references
References 10 publications
0
0
0
Order By: Relevance

No citations

Set email alert for when this publication receives citations?