“…2(a) presents an example of the dependence of the Curie temperature on the spacer thickness calculated either for the ideal surface and interface or for r ¼ 0:1: In Fig. 2(b) a similar comparison is presented for the case of thickness dependence of the spin-wave parameter B [7], which is the proportionality factor in the T 3=2 law for magnetisation in low temperatures. One can see that introducing of the roughness leads to decrease either in the amplitude of fluctuations of the Curie temperature or in the parameter B as a function of the spacer thickness.…”