Magnetostriction investigation of soft magnetic microwires

Abstract: The values of the magnetostriction constant, l s , of Co-based glass-coated microwires have been investigated by using the small-angle magnetization rotation (SAMR) method. Performing the systematic measurements, we were able to choose the appropriate measurement conditions achieving a highprecision result. From the dependence of the evaluated magnetostriction coefficient on annealing conditions, we evaluated the influence of the internal stresses on the magnetostriction coefficient value and the influence of … Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

1
59
0
1

Year Published

2017
2017
2023
2023

Publication Types

Select...
5
3
1

Relationship

1
8

Authors

Journals

citations
Cited by 61 publications
(61 citation statements)
references
References 24 publications
1
59
0
1
Order By: Relevance
“…Furthermore, the magnetostriction coefficient, λ s , of the studied microwire, estimated using the SAMR method adapted for microwire research, as described elsewhere [31,54], gives a value of about λ s ≈ −0.3 × 10 −6 .…”
Section: Experimental Methodsmentioning
confidence: 99%
“…Furthermore, the magnetostriction coefficient, λ s , of the studied microwire, estimated using the SAMR method adapted for microwire research, as described elsewhere [31,54], gives a value of about λ s ≈ −0.3 × 10 −6 .…”
Section: Experimental Methodsmentioning
confidence: 99%
“…The magnetostriction coefficient, λs, of the studied microwire, was evaluated by the SAMR method recently adapted for microwire [54,55]. In this method λs -values are determined in the microwire saturated by an axial magnetic field, H. Simultaneously, low AC transverse field, Hc, generated by an AC electric current flowing along the microwire allows a reversible magnetization rotation.…”
Section: Experimental Methods and Materialsmentioning
confidence: 99%
“…In this method λs -values are determined in the microwire saturated by an axial magnetic field, H. Simultaneously, low AC transverse field, Hc, generated by an AC electric current flowing along the microwire allows a reversible magnetization rotation. More detailed SAMR method description and of the set-up adapted for evaluation of magnetostriction coefficient in microwires are provided elsewhere [54,55].…”
Section: Experimental Methods and Materialsmentioning
confidence: 99%
“…from λ s ¡5 ¢ 10 ¡6 at x 1, to λ s 38 ¢ 10 ¡6 at x 0.2. Nearly-zero λ s -values can be achieved at Co/Fe 70{5 [34,35].…”