“…Room temperature compression tests of Zr 74.9 Ti 10.5 Ni 14.6 nanostructure-dendrite composite show evident yielding and 6% plastic strain together with work hardening up to 1622 Mpa [18]. Furthermore, for quaternary components Zr 61 Al 12.2 Ni 5 Cu 21.8 , Zr 60.6 Al 13.6 Ni 7.5 Cu 18.3 and Zr 60 Al 15-Ni 10 Cu 15 have a fracture stress of about 1750e1800 Mpa and plasticity less than 1.8% under compression tests [17].…”