Mechanical properties and wear resistance of direct energy deposited Fe–12Mn–5Cr–1Ni-0.4C steel deposited on spheroidal graphite cast iron

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1

Citation Types

1
4
0

Year Published

2022
2022
2024
2024

Publication Types

Select...
8

Relationship

2
6

Authors

Journals

citations
Cited by 11 publications
(5 citation statements)
references
References 25 publications
1
4
0
Order By: Relevance
“…This was due to the strong austenite stabilization effect of Mn. A similar observation was made in the L-DED-processed HMnS with a manganese content of 12 wt.% [22]. For the HMnS with a manganese content higher than 24 % used in this study, Hufenbach et al [25] reported that the Fe-30Mn-1C-0.02S (wt.%) alloy deposited through a selective laser melting process also comprises γ-austenite as the main phase.…”
Section: Microstructuressupporting
confidence: 82%
See 2 more Smart Citations
“…This was due to the strong austenite stabilization effect of Mn. A similar observation was made in the L-DED-processed HMnS with a manganese content of 12 wt.% [22]. For the HMnS with a manganese content higher than 24 % used in this study, Hufenbach et al [25] reported that the Fe-30Mn-1C-0.02S (wt.%) alloy deposited through a selective laser melting process also comprises γ-austenite as the main phase.…”
Section: Microstructuressupporting
confidence: 82%
“…In a pervious study by the authors, HMnS with a manganese content of 12 wt.% was successfully fabricated by the L-DED process [22]. The results showed that L-DED can produce HMnS with a near defect-free microstructure, without any significant macroscopic segregation of Mn due to rapid solidification.…”
Section: Introductionmentioning
confidence: 99%
See 1 more Smart Citation
“…For the use of WAAM in the field of Ni-based superalloys, Chigilipalli et al [158] compared the wear behavior of printed samples with wrought references and were able to demonstrate increased hardness as well as wear resistance in dry sliding wear tests. In [159], the DED process was also used to create a coating on a substrate surface. The substrate used was cast iron, on which a high-manganese steel was deposited.…”
Section: Direct Energy Deposition (Ded)mentioning
confidence: 99%
“…Ductile iron is a type of material with perfect castability, easy machinability, wear resistance, high strength to low weight ratio, fatigue strength, high corrosion resistance and toughness. Due to these properties, it is a widely used material in the machinery and automobile industries for structural components such as machine tool bearings, bearings, rolling mills, pistons, cylinders and pump housings [3].…”
Section: Introductionmentioning
confidence: 99%