Abstract:Pb2MgWO6 was prepared using mechanochemical activation and sintering in a temperature range of 600-1000ºÑ in three ways: 1) from oxides of the corresponding metals, 2) using MgWO4 precursor; and 3) in the presence of over-stoichiometric amounts (1wt.% and 2wt.% ) of Li2CO3 alloying additive.
Set email alert for when this publication receives citations?
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.