2011
DOI: 10.1016/j.matdes.2010.10.003
|View full text |Cite
|
Sign up to set email alerts
|

Microtensile testing of a free-standing Pt-aluminide bond coat

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1

Citation Types

0
20
0

Year Published

2011
2011
2022
2022

Publication Types

Select...
5

Relationship

2
3

Authors

Journals

citations
Cited by 19 publications
(20 citation statements)
references
References 20 publications
0
20
0
Order By: Relevance
“…The design of the specimen was based on a two-dimensional linear elastic finite element simulation, reported elsewhere. [34] For preparation of the specimens, strips of 0.5-mm thickness were first sliced from CM-247LC rods by wire-cut electodischarge machining (EDM). The PtAl coating was then applied on these strips in the manner mentioned previously.…”
Section: Methodsmentioning
confidence: 99%
See 1 more Smart Citation
“…The design of the specimen was based on a two-dimensional linear elastic finite element simulation, reported elsewhere. [34] For preparation of the specimens, strips of 0.5-mm thickness were first sliced from CM-247LC rods by wire-cut electodischarge machining (EDM). The PtAl coating was then applied on these strips in the manner mentioned previously.…”
Section: Methodsmentioning
confidence: 99%
“…[4,[23][24][25] In the present article, the effect of cyclic oxidation exposure [in air at 1373 K (1100°C)] on the tensile properties of DS Ni-base superalloy CM-247LC was examined in the PtAl bond coated condition. To achieve this, tensile testing of both bulk-coated samples and free-standing coating samples [33,34] was carried out. The tensile behavior of the coated alloy was correlated with the microstructural changes that occurred in the coating and the substrate during oxidation exposure.…”
Section: Introductionmentioning
confidence: 99%
“…The dimensions of the microsamples were established by a finite element method-based study. [10,11] The gage length (GL), gage width (GW), and fillet radius (R) of the cutout samples were 2, 0.5, and 0.5 mm, respectively, while their overall length was 8 mm, as shown in Figure 1(a). A holding length (HL) of 1 mm was provided in order to arrest the sample within slotted grips during testing.…”
mentioning
confidence: 99%
“…A holding length (HL) of 1 mm was provided in order to arrest the sample within slotted grips during testing. [7,10,11] The free-standing coating samples were prepared by precision polishing of the cut-out samples from one side until the substrate was completely removed and the sample thickness became equal to the thickness of bond coat, which was approximately 100 lm (Figures 1(a) and (b)). The flatness of the surface and uniformity in thickness reduction during polishing were ensured by the use of a Tripod Polisher.…”
mentioning
confidence: 99%