Monthly Progress Report for Chemical Development Section B (October 1958)

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1

Citation Types

0
4
0

Year Published

1960
1960
1960
1960

Publication Types

Select...
1

Relationship

0
1

Authors

Journals

citations
Cited by 1 publication
(4 citation statements)
references
References 0 publications
0
4
0
Order By: Relevance
“…Synthetic Zirflex decladding waste was heated with Ca(0H) 2 to volatilize ammonia and reduce the volume before adding sand and cement. The final cake had 23$ less volumes than the original waste and a compression test strength of 4200 psi.…”
Section: Intermediate Level Waste Treatmentmentioning
confidence: 99%
See 3 more Smart Citations
“…Synthetic Zirflex decladding waste was heated with Ca(0H) 2 to volatilize ammonia and reduce the volume before adding sand and cement. The final cake had 23$ less volumes than the original waste and a compression test strength of 4200 psi.…”
Section: Intermediate Level Waste Treatmentmentioning
confidence: 99%
“…The breakthrough curve in Fig. 17 indicates a decontamination factor of 10 4 for Cs 1^ (99-99$ removal) for the passage of 2k liters, 1490 column volumes, of waste.…”
Section: Kmentioning
confidence: 99%
See 2 more Smart Citations