“…Seldomly reported, the photocatalysts are susceptible to mechanical stress and eventual fracture caused by the stirring in the batch reactor, generating smaller particles and a higher surface area, which overestimates the photocatalytic performance and jeopardizes the claimed easy removal of the photocatalysts after a test. Also, porosity data, like specific surface area and pore diameter, are not properly discussed or even totally or partially missing in some papers in the literature [ 14 , 15 , 16 , 17 , 18 , 19 , 20 , 21 , 22 ], neglecting possible synergies and effects granted by the catalytic supports in what regards, e.g., mass transfer. Concerning the particle size, most of the reported microspherical supports are usually very small, ranging from 0.5 to 3 µm [ 18 , 19 , 20 , 21 , 23 , 24 , 25 ], which may impose problems and extra complexity and costs in a real-life application, in what regards the setup and recovery aspects.…”