“…From Figure (a), it remarked that the appearance of diffraction peaks (2 θ values) at 31.68°, 34.50°, 36.19°, 47.61°, 56.50°, 62.85°, 66.51°, 67.93°, 69.06°, 72.58°, and 76.81° related to the crystal planes (110), (002), (101), (102), (110), (103), (200), (112), (201), (004) and (104) correspondingly, and agree well with the data described in JCPDS no. 89–7102 . From these values, it validated that the ZnO nanoparticles maintain a wurtzite phase.…”