Nanoindentation measurements of combustion CVD Al2O3 and YSZ films

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

2
16
0

Year Published

2005
2005
2021
2021

Publication Types

Select...
7
2

Relationship

0
9

Authors

Journals

citations
Cited by 51 publications
(18 citation statements)
references
References 17 publications
2
16
0
Order By: Relevance
“…The techniques are expected to be useful for measurement of the mechanical properties of thin films or local structure of various materials. For example, the nanoindentation tests for MgO [8][9][10][11][12][13][14][15][16][17], TiO 2 [18,19], and YSZ [8,20,21] single crystals have been performed until now. However, there are few attempts to apply the nanoindentation to evaluate the mechanical properties of the nuclear fuels and materials.…”
Section: Introductionmentioning
confidence: 99%
“…The techniques are expected to be useful for measurement of the mechanical properties of thin films or local structure of various materials. For example, the nanoindentation tests for MgO [8][9][10][11][12][13][14][15][16][17], TiO 2 [18,19], and YSZ [8,20,21] single crystals have been performed until now. However, there are few attempts to apply the nanoindentation to evaluate the mechanical properties of the nuclear fuels and materials.…”
Section: Introductionmentioning
confidence: 99%
“…Chromia addition by itself did not help improve the properties significantly; however, it could act as a stabilizer for alumina and limit the phase transformations up to 1200°C ( Ref 46,58). Combination of SiO 2 and Al 2 O 3 can help improve high-temperature creep and corrosion resistance ( Ref 44,59,60). The creep measurements on hybrid spray coatings are in progress and will be reported elsewhere.…”
Section: Hot Corrosion Testmentioning
confidence: 99%
“…In other words, the samples coated by the laser technique are significantly more corrosion-resistant than the base materials. 4. Experiments involving oxidation in air, performed with TGA, indicated that laser-processed samples were more oxidation-resistant than were substrates.…”
Section: Research and Developmentmentioning
confidence: 99%
“…Therefore, large thermally induced mechanical stresses are set up in the interface regions. In the past, this problem was circumvented, though with limited technical or commercial success, through techniques such as diffusion coating, functionally gradient coating, and bond coatings via physical vapor deposition (PVD) [1][2][3], chemical vapor deposition (CVD) [4][5][6][7], thermal spraying [8][9][10][11], and weld overlay [12][13] techniques. Techniques such as diffusion coating have proven useful for producing coatings with good elevated-temperature properties.…”