Nickel Nitrate and Molybdenum Oxide as a Yttria-Stabilized Zirconia Synergistic Sintering Aid

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1

Citation Types

0
6
0

Year Published

2017
2017
2020
2020

Publication Types

Select...
2

Relationship

1
1

Authors

Journals

citations
Cited by 2 publications
(6 citation statements)
references
References 27 publications
0
6
0
Order By: Relevance
“…As shown in Figure 3c, stacks of perpendicularly grown plates were deposited on the substrate and the Raman spectra of these species verified the formation of various lower-valence-state Mo oxides 34,35 (see Figure S3d). Furthermore, the XRD data (Figure 3d) for the black-colored powder remaining in the boat indicated that most of the MoO 25,26 In Stage III (above 780 °C), the sulfur-induced transition to MoS 2 proceeds from the edges of the substrate to the center, as shown in Figure 2, demonstrating the possible dependence of this transition on the amount of sulfur supplied. Therefore, an increase in the number of MoS 2 atomic layers is expected upon increasing the sulfurization time in Stage III.…”
Section: ■ Results and Discussionmentioning
confidence: 95%
See 2 more Smart Citations
“…As shown in Figure 3c, stacks of perpendicularly grown plates were deposited on the substrate and the Raman spectra of these species verified the formation of various lower-valence-state Mo oxides 34,35 (see Figure S3d). Furthermore, the XRD data (Figure 3d) for the black-colored powder remaining in the boat indicated that most of the MoO 25,26 In Stage III (above 780 °C), the sulfur-induced transition to MoS 2 proceeds from the edges of the substrate to the center, as shown in Figure 2, demonstrating the possible dependence of this transition on the amount of sulfur supplied. Therefore, an increase in the number of MoS 2 atomic layers is expected upon increasing the sulfurization time in Stage III.…”
Section: ■ Results and Discussionmentioning
confidence: 95%
“…With progress of the CVD process, melting of the sulfur powder was initiated (at a CVD temperature over 680 °C, which corresponds to a temperature exceeding 105 °C at the site of the sulfur-containing boat), and the reaction zone quickly changed to a highly reducing atmosphere under a sufficient sulfur-vapor supply. Under these highly reducing conditions, it was expected that most of the deposited MoO 3– x would be quickly transformed to a nonvolatile compound such as MoO 2 before resubliming, given that the ramping rate (>50 °C min –1 ) was much higher than that used for conventional CVD processes (generally, <20 °C min –1 ). , …”
Section: Results and Discussionmentioning
confidence: 99%
See 1 more Smart Citation
“…Table 1. Green density, final sintered density, and maximum sintering rate; density measurements are relative to 5.9 g/cm 3 and given as a percent of theoretical density, and sintering rate as change in percent relative density per minute (%/min) (Adapted from [32]). The resistance term of this ubiquitous law is given as exp(−Q/RT).…”
Section: Resultsmentioning
confidence: 99%
“…(D) Ni(NO 3 ) 2 infiltrated 8YSZ with 10 mol.% MoO 2, where all samples were sintered up to and held at 1200 • C for one hour. From[32] with copyright permission.…”
mentioning
confidence: 99%