“…In order to achieve β-phase enhancement in PVDF/ ceramics nanocomposites, two core issues need to be considered: uniform dispersion of ceramics nanoparticles in the PVDF matrix and strong interfacial bonding between the ceramics and the PVDF [18,21]. In recent years, much effort has been made to obtain nanocomposites with nanoparticles' homogeneous dispersion, including surface modification by organic molecules such as rialkoxysilane [22], hydrogen peroxide [23], and hyperbranched aromatic polyamide [24], and the use of hybrid nanofillers such as siliver [17], nickel [25], and carbon material [26], and surface-initiated in situ polymerization [27,28]. However, these methods involved the usage of abundant solvents, which are unhealthy and environmentally unfriendly [29].…”