“…In general, increasing FRP amount was expected to develop more notable nonlinear responses, fracture skins at a higher stress and achieve a larger ultimate strain. to calculate the required strip width for FRP skins [12]. The strip widths were therefore 10 mm, 15 mm and 20 mm for the corresponding composites having 2 mm, 3 mm and 4 mm-height cores, respectively.…”