Oblique cross-section nanoindentation for determining the hardness change in ion-irradiated steel

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1

Citation Types

1
22
0

Year Published

2020
2020
2023
2023

Publication Types

Select...
6

Relationship

2
4

Authors

Journals

citations
Cited by 33 publications
(23 citation statements)
references
References 40 publications
1
22
0
Order By: Relevance
“…This was achieved after aligning all the samples to the reference of zero depth at the first indent on the epoxy-sample interface. The resulting ΔH-depth profiles for the sample irradiated with 1, 2, and 3 MeV He to a fluence of 1 × 10 17 ions/cm 2 are given in Figure 4b [15]. Some observations that can be made from this graph are:…”
Section: 'Oblique Cross-section' Indentation Methodsmentioning
confidence: 96%
See 4 more Smart Citations
“…This was achieved after aligning all the samples to the reference of zero depth at the first indent on the epoxy-sample interface. The resulting ΔH-depth profiles for the sample irradiated with 1, 2, and 3 MeV He to a fluence of 1 × 10 17 ions/cm 2 are given in Figure 4b [15]. Some observations that can be made from this graph are:…”
Section: 'Oblique Cross-section' Indentation Methodsmentioning
confidence: 96%
“…The model results underestimate the hardness in the shoulder region with a larger gradient close to the metal-epoxy interface. The model captures the position and magnitude of the peak hardness accurately after correction of the ISE of the unirradiated region as per the work of Pöhl et al [24] and outlined in the author's earlier study [15]. Conversely, for the top-down method, Figure 8b, we observe a broad hardness peak, both in the experiments and the simulation results, whereby the model slightly over-predicts the depth position at peak hardness (100-130 nm) and the magnitude of the hardness difference.…”
Section: Finite Element Modellingmentioning
confidence: 95%
See 3 more Smart Citations