“…The absence of Al shows that at the optimal ratio of Al and Fe, the volume fraction of the intermetallic can be increased up to 100%. Samples alloyed with Co were sintered under the same conditions [ 96 ]. After SPS in the materials containing Fe, Co and Al, several phases, such as FeAl, Fe 3 Al, FeAl 2 and FeCo increase the microstrains in the material [ 21 , 96 , 98 ] while γ-Fe and Co are responsible for an increased plasticity.…”